Choosing a tungsten carbide grade is rarely about finding the hardest material. The right grade is the one that lasts longest under your conditions without chipping, cracking or wearing out early. This guide gives you a simple way to narrow the choice before you talk to an engineer.
Start with how the part fails
If you are replacing an existing part, the worn part tells you a lot. The failure mode points to the property you need more of.
| What you see | What it suggests | Usual direction |
|---|---|---|
| Smooth, even wear | Abrasion is the main problem | A harder grade: lower cobalt, finer grain |
| Chipped edges | Impact or edge stress exceeds toughness | A tougher grade: more cobalt, or a stronger edge design |
| Cracks or sudden fracture | Heavy impact, or high tensile or bending load | A tougher grade, and a review of the part design |
| Pitting or a rough surface in fluid | Possible corrosion or erosion | Share the fluid and operating conditions before choosing a grade |
Describe the working conditions
Hardness and toughness pull in opposite directions, so a grade can only be judged against the job. These details matter most:
- Load type: steady sliding contact, repeated impact or high compressive load.
- Abrasive or workpiece material: what the part touches, and how hard or abrasive it is.
- Temperature and fluids: working temperature, coolant and any corrosive media.
- Part geometry: sharp edges and thin sections generally need more care than solid, rounded shapes.
Match the application to a grade family
The examples below show typical properties from the MOSCARB grade table. They are a starting point, not a final recommendation.
| Application | Example grade | Co (%) | Grain size (μm) | Hardness (HRA) | TRS (N/mm²) |
|---|---|---|---|---|---|
| Precision finishing rods | MU10UF | 6 | 0.4 | 94 | 3800 |
| Solid carbide tool rods | MU20 | 10 | 0.7 | 91.8 | 3800 |
| Custom wear parts | YG8 | 8 | 1.5 | 90 | 2900 |
| Cold heading dies | MCG5 | 12 | Medium | 88.3 | 3300 |
| Stamping dies | YG20 | 20 | 1.5 | 85 | 2500 |
The pattern is easy to see. Grades for fine cutting edges favor high hardness and very fine grain, while grades for forming and stamping give up hardness in exchange for resistance to repeated impact.
Use ISO ranges as a guide only
ISO application ranges such as K10 or K20 are helpful for a first comparison, but they are not exact specifications. Two grades in the same range can perform differently, so compare the cobalt content, grain size, hardness and transverse rupture strength as well.
Confirm the grade before production
Published properties are typical values. For a demanding application, the safest route is to share your drawing and operating conditions, confirm the grade with an engineer, and test a small batch before committing to volume.
Send your drawing and operating conditions and our engineers will review them and reply with questions or a grade suggestion.