How to Choose a Tungsten Carbide Grade for Your Application

Choosing a tungsten carbide grade is rarely about finding the hardest material. The right grade is the one that lasts longest under your conditions without chipping, cracking or wearing out early. This guide gives you a simple way to narrow the choice before you talk to an engineer.

Start with how the part fails

If you are replacing an existing part, the worn part tells you a lot. The failure mode points to the property you need more of.

What you seeWhat it suggestsUsual direction
Smooth, even wearAbrasion is the main problemA harder grade: lower cobalt, finer grain
Chipped edgesImpact or edge stress exceeds toughnessA tougher grade: more cobalt, or a stronger edge design
Cracks or sudden fractureHeavy impact, or high tensile or bending loadA tougher grade, and a review of the part design
Pitting or a rough surface in fluidPossible corrosion or erosionShare the fluid and operating conditions before choosing a grade

Describe the working conditions

Hardness and toughness pull in opposite directions, so a grade can only be judged against the job. These details matter most:

  • Load type: steady sliding contact, repeated impact or high compressive load.
  • Abrasive or workpiece material: what the part touches, and how hard or abrasive it is.
  • Temperature and fluids: working temperature, coolant and any corrosive media.
  • Part geometry: sharp edges and thin sections generally need more care than solid, rounded shapes.

Match the application to a grade family

The examples below show typical properties from the MOSCARB grade table. They are a starting point, not a final recommendation.

ApplicationExample gradeCo (%)Grain size (μm)Hardness (HRA)TRS (N/mm²)
Precision finishing rodsMU10UF60.4943800
Solid carbide tool rodsMU20100.791.83800
Custom wear partsYG881.5902900
Cold heading diesMCG512Medium88.33300
Stamping diesYG20201.5852500

The pattern is easy to see. Grades for fine cutting edges favor high hardness and very fine grain, while grades for forming and stamping give up hardness in exchange for resistance to repeated impact.

Use ISO ranges as a guide only

ISO application ranges such as K10 or K20 are helpful for a first comparison, but they are not exact specifications. Two grades in the same range can perform differently, so compare the cobalt content, grain size, hardness and transverse rupture strength as well.

Confirm the grade before production

Published properties are typical values. For a demanding application, the safest route is to share your drawing and operating conditions, confirm the grade with an engineer, and test a small batch before committing to volume.

Send your drawing and operating conditions and our engineers will review them and reply with questions or a grade suggestion.

Request a Quote

Send Your Drawing for a Manufacturing Review

Tell us what you need and our engineers will review it and reply with questions or a quotation.

Request a Quote →

For a faster quotation, include:

  • Drawing (PDF) or main dimensions
  • Tolerances and surface requirements
  • Preferred grade or operating conditions
  • Quantity and delivery schedule